Performance Material · Copper-Nickel Alloys
Navinic 10
CuNi10Fe1Mn · UNS C70600 | C70610 | C70620 | 7060X
Navinic 10: Copper-Nickel Alloys from the Lebronze Alloys North American range.
ASTM B466EEMUA 234BS 2871BS 2874CN 102
✓ Lead-free · REACH / RoHSOverview
Copper-Nickel Alloys.
Navinic 10: Copper-Nickel Alloys from the Lebronze Alloys North American range.
Sectors served
FamilyCopper-Nickel Alloys
CompositionCuNi10Fe1Mn
UNSC70600 | C70610 | C70620 | 7060X
TempersAnnealed / Cold worked
Density8.9 g/cm³
Conductivity9 %IACS
MagneticNo
FormsBars, Tubes
Mechanical properties
Minimum guaranteed properties.
Minimum guaranteed values by grade and product form.
| Grade / spec | Form | Tensile (ksi) | Yield 0.2% (ksi) | Elong. (%) | Hardness (HB) | Hardness (HRC) | Compliant with |
|---|---|---|---|---|---|---|---|
| Navinic 10 - Annealed | Bars | 44 ksi | 16 ksi | 35 | 70 | n/a | EEMUA 234, BS 2871, BS 2874, CN 102, ASTM B466 |
| Navinic 10 - Cold worked | Bars | 51 ksi | 36 ksi | 15 | 100 | n/a | EEMUA 234, BS 2871, BS 2874, CN 102, ASTM B466 |
| Navinic 10 - Annealed | Tubes | 44 ksi | 16 ksi | 35 | 70 | n/a | EEMUA 234, BS 2871, BS 2874, CN 102, ASTM B466 |
Data for information only, non-contractual. Request a certified datasheet for design allowables.
Physical properties
| Density | 8.9 g/cm³ |
| Electrical conductivity | 9 %IACS |
| Thermal conductivity | 50 W/m·K |
| Young's modulus | 130 GPa |
| Thermal expansion | 17 ×10⁻⁶/K |
| Magnetic permeability | 1.01 |
| Machinability index | 20 |
| NACE corrosion rating | 5 |
Standards & specifications
Norms & designations.
Norms & designations
- ASTM B466
- EEMUA 234
- BS 2871
- BS 2874
- CN 102
Available forms
Forms & applications.
Available form
Bars
Available form
Tubes